| CHARACTERISTICS |
Test |
Results |
| Adherence by cut and grating |
UNE-EN-ISO 2409-96 |
OK |
| Resistance to Buchholz system |
UNE 48252 ISO 2815 |
OK |
| Resistance to inlay |
UNE-EN-ISO 1520-96 |
OK |
| Resistance to fold by cylinder mandrell |
UNE-EN-ISO 1519-96 |
IN AGREEMENT |
| Resistance test of sawing, drilling and milling
cutter. |
AIMME |
There isn't peeling or detachment of painting coat. |
| Resistance test to boiling water |
AIMME PE-C012 |
Without blistering |
| Test Machu |
AIMME PE-C024 |
Intact |
| Test of Polymerisation grado |
AIMME PE-C014 |
OK |
| Resistance test to damp |
UNE-EN-ISO 6270 |
Without corrosive process or loss adherence. |
| Kesternich Test (sulphur dioxide) |
UNE-EN-ISO 3231 |
Without corrosive process or loss adherence. |
| Test saline-oiled fog |
UNE-112-017-92
ISO 92227-90 |
Without corrosive process or loss adherence. |
| Resistance test of mortar |
AIMME PE-C011 |
No defect |
| Test Tabber abrasive |
ASTM-D-4060 |
20% more resistant than normal lacquer |
| Shine and colour variation 13/05/97 |
ISO-1134-94 |
|
| Accelerated to make it old by exposure to radiation
Xenon arch. |
ISO-2813 |
|
| Panels follow the test of accelerated
to make it old in the shine paragraph. Colour difference, because of the
decoration kind can´t be measured by chromatic coordinates and significative
the changes can´t be observed. The results obtained in the samples tested to the accelerated to make it old are: |
| Shine: Initial: 65% Final: 58% Residuary:
89% |